First, argon arc welding, precision castings, alloy steel, stainless steel casting, aluminum alloy die castings with argon arc welding machine for welding repair.Part of the mould manufacturing and repair factory, also USES the welding repair mold defect.Advantages: welding repair of high efficiency, high precision of the electric welding machine.Wire sort is more, the most widely used on stainless steel, aluminum alloy products.Can be used for welding, high intensity of teaching.Disadvantages: used for defect repair, small defect fix (porosity, sand holes), because of the impact is too large, the molten pool line trace (bite edge phenomenon).Weld steel has a hard point.Due to thermal effects, non-ferrous casting or thin-walled weld repairs, easy to produce thermal deformation.Operating higher technical requirements.
Three methods can eliminate the casting defects
Second, electric welding machine, cast iron, cast steel weld with traditional way.Advantages: repair defects, high efficiency.Disadvantages: solder joints on high hardness after welding, internal stress, prone to cracks, general need annealing heat treatment can meet the requirements of processing.And limit because of the welding condition, internal easy to produce the secondary defects such as porosity, slag.
Three methods can eliminate the casting defects
Third, argon arc welding, precision castings, alloy steel, stainless steel casting, aluminum alloy die castings with argon arc welding machine for welding repair.Part of the mould manufacturing and repair factory, also USES the welding repair mold defect.Advantages: welding repair of high efficiency, high precision of the electric welding machine.Wire sort is more, the most widely used on stainless steel, aluminum alloy products.Can be used for welding, high intensity of teaching.Disadvantages: used for defect repair, small defect fix (porosity, sand holes), because of the impact is too large, the molten pool line trace (bite edge phenomenon).Weld steel has a hard point.Due to thermal effects, non-ferrous casting or thin-walled weld repairs, easy to produce thermal deformation.Operating higher technical requirements.
 

  • Q Are you a manufacturer or a trader?

    A
    We have our own foundry ,forging factory and machinery shop located in Liaoning Province, China.
  • Q What can you do for customer?

    A
    One Stop Service
    1).Manufacturing and supply various machinery parts.
    2). Technical analysis and design 
    3).Factory audit, on-site production supervision, in-time feedback, pre-shipment quality inspection
  • Q How could you commit the product quality?

    A
    1) all our factories were ISO certified. 
    2) more than 50% of New Densen’s products were sold to worldwide top 500 companies 
    which located in North American, Western Europe, and Japan.
    3) New Densen’s QC engineers will do on-site supervision and before EX-work quality inspection. New Densen will issue inspection reports for customers’ approval before EX-work. New Densen will be responsible for its reports and every parts no matter how long sold to customers.
  • Q How long shall we get the quotation?

    A
    Processing time for inquiry: 1-3 working days.
  • Q What's the process of developing a new steel casting product?

    A
    The procedure for new project develop as below:
    1. Technical department analyze the drawings all details 
     
    2.Pattern design and manufacture
     
    3.Casting Process
     
    4.Quality Control inspect the casting parts
     
    5.Issue inspection report for customer to check quality
     
    6. After inspection report approved, Logistics Department help arrange the shipping to customer