contact@sydensen.com    |        +86 155 4152 4932
Floor 20, Block B, Fortune Building, No. 18 Xinghua Bei Street , Tiexi District, Shenyang, 110025, China.

Steel pressure vessel welding procedure qualification conditions

Views: 19     Author: Site Editor     Publish Time: 2016-10-27      Origin: Site

facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
kakao sharing button
snapchat sharing button
telegram sharing button
sharethis sharing button

Steel pressure vessel welding procedure qualification of general provisions, you may have not been very clear, let's take a look at.
Steel pressure vessel welding procedure qualification conditions
1, the welding procedure qualification should be based on reliable steel welding performance, and completed before the product welding.
2, general welding procedure qualification process are: welding process procedure and welding specimens and test, the test specimen and the specimen, determine whether welding joint has required the use of performance, make the welding procedure qualification report to assess the proposed welding process instructions.Welding procedure qualification test welds unit the correctness of the proposed welding process, welding unit capacity and evaluation.
3, the cross section of the penetration of T joint and the joint Angle, when unable to detect internal defects, and manufacturing units do not have enough ability to ensure that the weld penetration, should add production type testing of welding procedure qualification, confirmed by the dissection test can allows the welding products.
4 used equipment, instrumentation, welding procedure qualification should be in normal working state, steel, welding materials must conform to the corresponding standards, by this unit skilled welding workers have been using this unit welding equipment welding specimen.
Steel pressure vessel welding procedure qualification conditions
The above is the welding procedure qualification for steel pressure vessel conditions of related introduction, hope can help to you.

Related Products

content is empty!

     contact@sydensen.com
 
   Floor 20, Block B, Fortune Building, No. 18 Xinghua Bei Street , Tiexi District, Shenyang, 110025, China.
 
   +86-15541524932
FOLLOW US
Copyright © Densen Group, All Rights Reserved.
Leave a Message
message